• ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard

ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard

商品の詳細:

起源の場所: 中国湖南

お支払配送条件:

最小注文数量: 100
価格: $9-20
ベストプライス 連絡先

詳細情報

化学組成: アル 材料: アルミニウム
Alの内容: アルミ合金 合金タイプ: アル-Zn-イン合金
Znの内容: 2.5~7.0% コンテンツ内: 0.018~0.050%
CDコンテンツ: 0.005~0.020% SN含有量: 0.018~0.075%
Mgの内容: 0.50~1.50% Siの内容: 0.10~0.15%
チタニウムの内容: 0.01-0.08% Open-circuit電圧: -1.18 ~ -1.10V
閉回路電圧: -1.12~-1.05V 実際の容量: ≧2400Ah/kg
現在の効率: 85%以上
ハイライト:

ISO9001:2008 Certified Sacrificial Aluminum Anode

,

GB/T 4948-2002 Standard Aluminum Bracelet Anode

,

Galvanic Corrosion Protection Aluminum Alloy Anode

製品の説明

Sacrificial Aluminum Bracelet Anodes for Galvanic Corrosion
Sacrificial bracelet anodes are typically made from either zinc alloy or aluminum alloy, depending on design requirements, environmental variables, and water salinity. These anodes provide cost-effective and reliable cathodic protection for submerged pipelines, which are usually coated with anti-corrosion materials and weighted with concrete for negative buoyancy.
Bracelet anodes are mounted at specific locations determined by the cathodic protection system design and are electrically connected to the pipeline via special bonding copper cables. While the primary defense against corrosion is the pipeline's anti-corrosion coating, bracelet anodes protect areas where coating failures may occur during installation or operation.
Sacrificial Aluminum Bracelet Anodes mounted on pipeline Close-up view of Sacrificial Aluminum Bracelet Anodes
Applications
These anodes are used for:
  • Hull protection
  • Ballast tanks
  • Offshore engineering
  • Harbor structures
  • Sea water cooling systems
  • Submerged pipelines
Chemical Composition Standards
Type Zn In Cd Sn Mg Si Ti Impurity (less than) Al
Al-Zn-In-Cd A11 2.5-4.5 0.018-0.050 0.005-0.020 - - -- - 0.10 Balance
Al-Zn-In-Sn A12 2.2-5.2 0.020-0.045 - 0.018-0.035 - - - 0.10 Balance
Al-Zn-In-Si A13 5.5-7.0 0.025-0.035 - - - 0.10-0.15 - 0.10 Balance
Al-Zn-In-Sn-Mg A14 2.5-4.0 0.020-0.050 - 0.025-0.075 0.50-1.00 - - 0.10 Balance
Al-Zn-In-Mg-Ti A21 4.0-7.0 0.02-0.050 - - 0.50-1.50 - 0.01-0.08 0.10 Balance
Electrochemical Characteristics
Item Material of anodes Open-circuit Voltage (v) Close-circuit Voltage (v) Actual Capacity(Ah/kg) Current efficiency (%) Consumption rate (kg.(A.a)) Dissolve Performance
Electrochemical Performance Type 1 -1.18- -1.10 -1.12- -1.05 ≥ 2400 ≥ 85 ≤ 3.65 The surface dissolve evenly & oxide drop easily
Type 2 -1.18- -1.10 -1.12- -1.05 ≥ 2600 ≥ 90 ≤ 3.37
Reference electrode: Saturated calomel electrode
Type 1: A11, A12, A13, A14
Type 2: A21
Why Choose Us?
Q. Why choose us?

A. We have over 20 years of experience in the cathodic protection anode market. Our products are strictly produced and tested according to American standard ASTM G97, ensuring continuous and stable high quality that saves you costs.

B. We offer prompt shipment. For urgent needs, we maintain stock of regular shape anodes to enable quick delivery, even when standard plant delivery time is 20 days.

Our sales office Our manufacturing workshop
Company Culture
  • Our Belief: Continuous Innovation
  • Our Spirit: Sincerity, Unity, Dedicated, Hardworking
  • Our Mission: Provide most advanced products & most professional technical solution
Certification
Our product certifications
Inspection & Lab
Our inspection and laboratory facilities

この製品の詳細を知りたい
に興味があります ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard タイプ、サイズ、数量、素材などの詳細を送っていただけませんか。
ありがとう!
お返事を待って。